Place of Origin: | Liaoning |
---|
Location: | Anshan, Liaoning, China (Mainland) |
---|---|
Business Type: | Manufacturer, Trading Company |
Alloy steel
|
The similar grades of foreign countries
|
China
4Cr5MoSiV1 |
America
H13 |
Japan
SKD61 |
German
X40CrMoV51 (1.2344) |
Bohler
W302 |
||||||||||||||||||
Chemical component (%)
|
|
||||||||||||||||||||||
Specialty
|
Harden and air cooling steel, 600`C work, high rigidity, high endurance, anti-heating, anti-cracking, electric sediment and middle-melting steel, compact structure, refined in electric cooker, quality of steel is pure, owned good character of equal direction
|
||||||||||||||||||||||
Use
|
Extrusion mold of aluminum and magnesium, die-casting mold, especially adapt to the mold in large and complicated form.
|
||||||||||||||||||||||
Extrusion mold of copper alloy, die-casting mold
|
|||||||||||||||||||||||
Hot pressing machine mold
|
|||||||||||||||||||||||
Heat treatment
|
Quench:1000-1040`C via 600`C and 850`C, preheating oil or wind cooling
|
||||||||||||||||||||||
Temper temperature and rigidity HBC(reference)
|
|||||||||||||||||||||||
|
|||||||||||||||||||||||
Temper temperature should be higher than working temperature in order to stabilize the working size of mold
|
|||||||||||||||||||||||
Heat up to 650`C of average temperature in order to eliminate the machined stress, 500`C air cooling after electric cooker cooling
|
|||||||||||||||||||||||
Tempering, 800-850`C,slow cooling after diathermia
|
|||||||||||||||||||||||
Dimension(mm)
|
Round: ?0-?00 Flat :20-80*40-800 80-300*500-800
|
||||||||||||||||||||||
The state of leaving factory
|
HBS<=235
|