user login

Bridge Expansion Joint Concrete Repair Products

1800.0 USD
Min. Order: 5 Short Ton
Trade Term: FOB
Payment Terms: L/C, D/P, D/A, T/T, WU
Supply Ability: 1000 tons / month
Place of Origin: Henan

Company Profile

Location: Zhengzhou, Henan, China (Mainland)
Business Type: Manufacturer, Trading Company
Main Products: Concrete Repaid Repair Materials, Concrete Driveway Crack Repair Materials, Best Concrete Waterproof Repair Mortar, Best Material For Filling Cracks In Concrete Driveway, Bridge Deck Expansion Joint Repair Solution

Product Detail

Model No.: QM
Means of Transport: Ocean
Brand Name: HUINENG
Usage: Repair expansion joint concrete
Initial setting: 25mins
Final setting: 35mins
Compressive strength: 33.0Mpa/ 2 hours
Pulling strength: 2.8Mpa
Expansion rate: 0.01%
Open traffic time: 2 hour
Color: Grey
Certificate: ISO9001
Inspection report: MSDS
Production Capacity: 1000 tons / month
Packing: 25kg/bag
Delivery Date: in one week
Show

Product Description

       Bridge Expansion Joint Concrete Repair Products


There are many damages on bridge expansion joint concrete, 

such as: cracks, potholes, broken,exposed reinforcing bar etc.


Detailed repair solution:

1: which kind repair material is best for expansion joint concrete broken?

Huineng brand QM type concrete repair material is very suitable for repair expansion joint concrete cracks, potholes,

broken, exposed reinforcing bar,edge failure etc damages. rapid setting, 1 hour open to traffic.

2: why QM type concrete repair material is suitable?

1)1h open to traffic:

Fast with strength,2h compressive strength ≥33Mpa, 2h flexural strength ≥5Mpa,

Fully meet bridge rapid repairing,reduce traffic congestion.

2)Bonding tightly: No break and fall off from normal concrete under heavy load.

3)High strength: Compressive and flexural strength in late period, both reach 2-3 times of normal concrete. Compressive strength:1d≥60Mpa, 28d≥80Mpa,Flexural strength ≥10Mpa.

4)Good toughness:Impact resistance strength is 8-10 times of normal concrete

impact resistance strength

5)No drying cracks in repaired area and original concrete 

6)Good match:Heat expansion and cold contraction coefficient is nearly same with original concrete.

7)Small color difference: Color of repaired area is close to original concrete.

8)Fast repair: 

Just need chisel damage area accurately,produce less waste, high efficiency, road closed time is short.

3: what is the testing data?

Test items 

Unit

Technical requirement

Test result 

Individual conclusion

Setting time

Initial setting

Min

≥20

  25

Meet requirement

Final setting 

≤60

  35

Compressive strength

2h

Mpa

≥20

  33.0

Meet requirement

1d

≥40

  66.1

28d

≥50

  90.5

Flexural strength

2h


     ≥4

  5.5

Meet requirement

1d

     ≥6

  10.5

28d

     ≥8

  13.5

Pulling strength

28d

Mpa

     ≥2.0

   2.8

Meet requirement

Expansion rate

28d

 /

0.00%-0.1%

   0.01%

Meet requirement