user login

Repair Lacquer Interior Wall Putty For Mosaic Tile , Non Toxic

Place of Origin: Zhejiang

Company Profile

Location: Guangzhou, Guangdong, China (Mainland)
Business Type: Manufacturer
Main Products: Ceramic Wall Tile Adhesive, Ceramic Floor Tile Adhesive, Marble Tile Adhesive

Product Detail

Model No.: PB-08

Product Description

 

Repair Lacquer Interior Wall Putty For Mosaic Tile , Non Toxic

 

 

Features:

 

This product is directing at the application of the high-level exterior wall putty and specially developed high-level exterior wall putty, provides a flat base surface and has strong bonding power to the coating.

1, Strong bonding power, can be well attached to the wall and coating.

2, Good thixotropy, can form a nearly-perfect smooth surface by simply floated, reduce the loss caused by pasting excessively due to the uneven surface.

3, Good anti-crack function . 

4, Good damp-proof and ventilation function and keep the wall and the painting dry.

5, Good flexibility, can resist the damage of temperature, ensure the long-term decoration effect of the painting.

6, Natural texture, ensure that the decorative effect can be completely reflected. 

 

 

Application:

 

1, The paint bottom ash on the new and old walls.

2, The paint bottom ash retreaded directly on the old surface (paint, tile, mosaic, stone and other smooth surface).

3, More suitable for the basic layer skim coat of the imitation aluminum, the metallic paint,etc.

 

 

Operation Process:

 

1, The ratio: powder: water: additive=8: (2~2.8): 1(25kg  powder: 5kg water: 2.0kg additive).

2, The substrate surface should be firm, dry and clean, no grease, no wax, and other loose materials.

3, If the wall is too dry, wet the wall till there is no obvious water on the surface before operation.  

4, Pouring the water into the container, and adding the powder slowly, then stirring them into a uniform, no-powder and no- deposit paste. Using inserting tools to insert, making the second time 4~6h after the first inserting. Polishing the skim coat layer, control the thickness between 0.8~1.5mm.

5, During the inserting process, make sure it is even and has no flaws.

6, When finishing the putty layer, polish within 1~2 days according to the weather.

7, Can paste other coating 7 days after finishing the skim coat layer. But using anti-alkali base coat can shorten the time.

 

 

Technical Reference:

 

Shrinkage(%)

≤0.5MPa

Tensile strength resistance to temperature

≥1.2MPa

Compression and shear bond strength

≥1.5MPa

Tensile strength resistance to freezing and thawing

≥1.0MPa

Waterproofing pressure strength

≥1.2MPa

Resistance to artificial aging strength(1000h)

No peeling, no crack, no peeling

 

 

Normal Amount:

 

Thickness under 1.5mm, about 1.8~2.5kg/.

 

 

Cautions:

 

1, Make sure the smooth and vertical rate of the surface before operation.

2, Never mix the dry slurry with water for second use.

3, The mixed skim coat should be used up within 3h.

4, Operating in the situation under 5~40, and never operate under rain.

5, After finished the skim coat layer, do the polishing within 7 days or it will be difficult for later polishing, maintaining for 2~3 days with water can get a better effect for the layer hardness.

6, For the uneven surface, suggesting dealing it with PB Base Skim Coat first.

 

 

Store Method:

 

Store in cool and dry place, unopened product can be saved for one year.

 

 

Packing:

 

20kg/bag

Post Buying Request