user login

MMO Wire Anode from China Manufacturer

1.0 USD
Min. Order: 1 Meter
Trade Term: FOB,CFR,CIF,DAT,FAS,DAP,CIP,CPT,FCA,EXW,DDU
Payment Terms: Paypal, L/C, T/T, WU
Supply Ability: 5000m per day
Place of Origin: Shaanxi

Company Profile

Location: Xi'an, Shaanxi, China (Mainland)
Business Type: Manufacturer

Product Detail

Model No.: TJW
Means of Transport: Ocean, Air, Land
Brand Name: Taijin
Substrate: Titanium ASTM B348 Gr1
Catalyst: Mixed Metal Oxide
Coating: IrO2/Ta2O2
Coating uniformity: Greater than 90 percent
Application enviroment: soils, freshwater, brackish water and seawater
Electrical Resistance: 1.5mm Dia Wire-0.248 ohms/m,3.0mm Dia Wire-0.248 ohms/m
Working life: Min.20 years
Quality control: Confirm to system standard ISO9001:2008
Stock: 2000m-finished products, 10000m-half-finished products
Accelerated Life Test of MMO Wire Anodes: 1mol Na2SO4, Current 10000A/m2, Accelerated life/Strenthening life>73 days
Production Capacity: 5000m per day
Packing: Inner package: soft paper, Outer package: plswood case
Delivery Date: According to the client's requirmen t(min.2 days)
Show

Product Description

MMO Wire Anode

 

 

※ MMO Wire Anode are manufactured using solid titanium, which meets ASTM B863 Grade 1 or Grade 2 standards, which has been coated with Taijin Mixed Metal Oxide coating. The mixed metal oxide is a crystalline, electrically conductive coating that activates the titanium and enables it to function as an anode.  

 

1)      SUBSTRATE

 

Titanium ASTM B 863 Grade 1 and Grade 2

 

2)      COATING

 

IrO2/Ta2O5

 

3)      SPECIFICATION & DIMENSIONS

   

Diameter(mm)

Length Per coil (m)

Working Life(y)

1.0

100,200,300

20

1.5

100,200,300

20

3.0

100,200

20

 

4)      PERFORMANCE DATA

 

Electrolyte

Max Current Density(A/m2)

Working Life

Soil

50A/m2 (4.6A/ft2)

20 years

Carbonaceous backfill

100A/m2(9.3 A/ft2)

20 years

Freshwater

100A/m2( 9.3A/ft2)

20 years

Brackish water

100-300A/m2(9.3A/ft2-27.8A/ft2)

20 years

Sea water

600 A/m2(55.8A/ft2)

20 years

Coating load can be adjusted depending on customers' particular design life and current density requirement

  • Current density should be determined in accordance with brackish water resistivity

 

5) QUALITY CONTROL

 

Strict quality procedures are followed throughout the whole process from raw materials to finished products to ensure coating adhesion and loading.

 

a)    Chemical Composition- ASTM B863 Gr1

b)    Visual Coating Uniformity, Color and Scratch

c)    Coating adhesion

 

Three Steps

 

 First, feeling the surface of tubular anodes in a pair of white gloves to observe whether black mark is left on the gloves

Second, paste with transparent tape to observe whether black mark is left on the Tape

Third, bend wire to observe whether the coating fades

 

d)    Accelerate Life Test

 

NACE standard TM0108-2008, 20000A/m2, 1mol/l Na2SO4, Accelerated Life Test Failure time: 35-40 days

 

6) WORKSHOP

 

 

 

 

6) LABORATARY

 

 

 

 

 

Post Buying Request