Min. Order: | 1 Meter |
---|---|
Trade Term: | FOB,CFR,CIF,DAT,FAS,DDP,DAP,CIP,CPT,FCA,EXW |
Payment Terms: | Paypal, L/C, T/T, Money Gram |
Supply Ability: | 5000m within 24 hours |
Place of Origin: | Shaanxi |
Location: | Xi'an, Shaanxi, China (Mainland) |
---|---|
Business Type: | Manufacturer |
Model No.: | TJM |
---|---|
Means of Transport: | Ocean, Air, Land |
Brand Name: | Taijin |
Substrate: | Titanium ASTM B265 Grade 1 |
Coating: | Noble mixed metal oxide consisting of IrO2 and Ta2O5 |
Coating Method: | Multi layer thermal decomposition of precious metal salts |
Working Environment: | Suitable for Cl2&O2or combination of both |
Working current: | 42mA /m when operating at an anode current density of 3 A/m2 |
Working life: | 50 years |
The 3rd party quality test: | Passed the quality test from USA DNV under the standard of NACE TM0108-2008 |
Lead time: | quick and the same as confirmed email |
Responding: | The 1st time to respond you when receiving your inquiry |
Price and shipping cost: | The most competitive price |
Production Capacity: | 5000m within 24 hours |
Packing: | Pls refer to the photos of package |
Delivery Date: | According to the Client's order volume(min.2 days) |
Titanium MMO Ribbon anode for CP of above ground storage tanks
1. Substrate& Coating
Titanium ASTM B265 Grade1
1)Composition
C | max 0.08% |
N | max 0.03% |
H | max 0.015% |
Fe | max 0.20% |
O | max 0.18% |
Residual | max each 0.1% |
Residual | max total 0.4% |
Ti | balance |
2)Coating:Mixed Metal Oxide-IrO2+Ta2O5
2. Dimensions &Parameters
Width(mm) Thickness Length CurrentOutput ExpectedLife(Y)
6.35 0.635 (mm) 155(m) 17(mA/m) 50
6.35 0.635(mm) 155(m) 43(mA/m) 50
3.Application
1) Under tank protection
2) Internal tankprotection
3) Aboveground storage tanks.
4.Producing Process
Raw material --- Cutting Ribbon--- Picking----Automatic coating---Inspection---Package
5. Quality Control & Assurance
Strict quality procedures are followed throughout the whole process from raw materials to finished products to ensure coating adhesion and loading.
1) Chemical Composition- ASTM B265 Gr1
Element | Content % |
Nitrogen | 0.03 Max |
Carbon | 0.08 Max |
Hydrogen | 0.015 Max |
Iron | 0.2 Max |
Oxygen | 0.18 Max |
Residual(each) | 0.1 Max |
Residual(total) | 0.4 Max |
Balance |
2) Visual Coating Uniformity, Color and Scratch
3) Coating adhesion
Three Steps
First, feeling the surface of tubular anodes in a pair of white gloves to observe
whether black mark is left on the gloves
Second, paste with transparent tape to observe whether black mark is left on the
Tape
Third, bend the ribbon to observe whether the coating fades
4) Accelerate Life Test
NACE standard TM0108-2008, 15000A/m2, 1mol/l Na2SO4
5. Workshop
Automatic and Continuous Ribbon Furnace
Accerlerate LifeTest
Coating Thickness Test
6.Products:
7. Engineering Pictures
MMO Ribbon Anode for Under tank CathodicProtection