user login

MMO Mesh Ribbon Anode Used for Cathodic Protection of Steel Rebar

1.0 USD
Min. Order: 1 Meter
Trade Term: FOB,CFR,CIF,DAT,FAS,DAP,CIP,CPT,FCA,EXW,DDU
Payment Terms: Paypal, L/C, T/T, WU, Money Gram
Supply Ability: 5000m/24 hours
Place of Origin: Shaanxi

Company Profile

Location: Xi'an, Shaanxi, China (Mainland)
Business Type: Manufacturer

Product Detail

Model No.: TJM
Means of Transport: Ocean, Air, Land
Brand Name: Taijin
Composition: Titanium ASTM B265 Gr1
Coating: Mixed Metal Oxide( Iridum base)
Expected life(NACE Standard TM02944-94): 100 years
Large Mesh Diamond: 25*50*0.89mm,35*75*0.89mm,24*60*0.89mm,16*40*0.89mm
Coil Length: 76m/coil
Accelerated Life: 1 mol/l Na2SO4, Current15000A/m2, Accelerated life>50 hours
Test Certificate: The third party test certificate from Det Norske Veritas (U.S.A.), Inc. , Evaluation Certificate from Bureau Veritas
Advantage 1: We are the earliest and biggest titanium manufacturer in China
Advantage 2: We will give customer shipping cost primage
Advantage 3: The quickest responding
Production Capacity: 5000m/24 hours
Packing: Plastic or paper as inside, carton or plywood case as outside
Delivery Date: 2 days to 15 days depend on the quantity
Show

Product Description

MMO Mesh Ribbon Anode

Mixed Metal Oxide (MMO) Mesh is a durable anode designed for ImpressedCurrent Cathodic Protection systems of steel structures and steel reinforcement concrete. The MMO coating, with industrially proven lifetime characteristics,ensures an even current distribution.

1. Substrate & Coating

1) Titanium ASTM B265 Grade 1

2)Coating: Mixed Metal Oxide-IrO2+Ta2O5

2.Parameters:

1)Other specification can be availableas client's requirement.

width

(mm)

length

(m)

thickness

(mm)

Current Rating

surface area

(m2)

mesh dimension

(mm)

10

76

1.3

2.8ma/m

1.85

2.5x4.6 x0.6

13

76

1.3

3.5ma/m

2.4

2.5x4.6 x0.6

19

76

1.3

5.28ma/m

3.6

2.5x4.6 x0.6

1220

76

1.98

37.8ma/m2

92.9

25x50 x0.89

1220

76

1.98

24.4ma/m2

92.9

34x76x0.89


2) Anode Performance:

Current Rating at 100 mA/m2(10mA/ft2)

2.8mA/m(0.085mA/ft)

Expected life(NACE Standard TM02944-94)

100years

Catalyst

Mixed Metal Oxide(MMO)

Maximum anode concrete interface current density:

FHWA limit

110mA/m2(10mA/ft2)

Short-term limit

220mA/m2(20mA/ft2)



3.Application


Reinforced concrete, Bridge,Pier Floodcontrolembankment;


4. The Third Party Certificate

                     Test Cetificates from Det Norske Veritas (U.S.A.), Inc. Under NACE TM0108-2008



Production Assessment from Bureau Veritas




5. Quality Assurance





  • Quality Assurance of MMO Mesh Ribbon

 

Strict quality procedures are followed throughout the whole process from raw materials to finished products to ensure coating adhesion and loading.

 

1)      Chemical Composition- ASTM B265 Gr1

 

Element

Content %

Nitrogen

0.03 Max

Carbon

0.08 Max

Hydrogen

0.015 Max

Iron

0.2 Max

Oxygen

0.18 Max

Residual(each)

0.1 Max

Residual(total)

0.4 Max

Titanium

Balance

 

2)      Visual Coating Uniformity, Color and Scratch

 

3)      Coating adhesion

 

Three Steps

 

 First, feeling the surface of tubular anodes in a pair of white gloves to observe

 whether black mark is left on the gloves

 

Second, paste with transparent tape to observe whether black mark is left on the

Tape

 

Third, bend the ribbon to observe whether the coating fades

 

4)      Accelerate Life Test

 

NACE standard TM0108-2008, 15000A/m2, 1mol/l Na2SO4

 


7. Quality Assurance of MMO Mesh Ribbon

 

Strict quality procedures are followed throughout the whole process from raw materials to finished products to ensure coating adhesion and loading.

 

1)      Chemical Composition- ASTM B265 Gr1

 

Element

Content %

Nitrogen

0.03 Max

Carbon

0.08 Max

Hydrogen

0.015 Max

Iron

0.2 Max

Oxygen

0.18 Max

Residual(each)

0.1 Max

Residual(total)

0.4 Max

Titanium

Balance

 

2)      Visual Coating Uniformity, Color and Scratch

 

3)      Coating adhesion

 

Three Steps

 

 First, feeling the surface of tubular anodes in a pair of white gloves to observe

 whether black mark is left on the gloves

 

Second, paste with transparent tape to observe whether black mark is left on the

Tape

 

Third, bend the ribbon to observe whether the coating fades

 

4)      Accelerate Life Test

 

NACE standard TM0108-2008, 15000A/m2, 1mol/l Na2SO4

 

8. Products

Raw Materials

MMO Coated Titanium Mesh Ribbon Anode


Half-finishedProducts

MMO Coated Titanium Mesh Ribbon Anode



MMO Coated Titanium Mesh Ribbon Anode

Finished Items




Packages


MMO Coated Titanium Mesh Ribbon Anode



 

 

 

 

Post Buying Request