user login

Chemical Industry double sphere rubber expansion joint

100.0 USD
Min. Order: 1 Piece/Pieces
Trade Term: FOB,CFR,CIF,DDP,DAP,EXW
Payment Terms: Paypal, L/C, D/P, D/A, T/T, WU, Money Gram
Supply Ability: 20000 Piece/Pieces per Month
Place of Origin: Hebei

Company Profile

Location: Cangzhou, Hebei, China (Mainland)
Business Type: Manufacturer, Trading Company
Main Products: Pipe, Fitting, Valve, Flange, Tee

Product Detail

Means of Transport: Ocean, Land
Head Code: Others
Shape: Equal
Technics: Casting
Type: Flange
Material: Others
Brand Name: stonefitting
Min.Order Quantity: 20 Set/Sets 2000USD
port: tianjin
place of orange: china
brand name: stonefitting
Material: Steel and Nature rubber
Production Capacity: 20000 Piece/Pieces per Month
Packing: Standard Export Package
Delivery Date: 15 days after getting the deposit
Show

Product Description

1.Rubber expansion joint Specifications

1.DN 32~3000mm 
2.PN 0.25/0.6/1.0/1.6/2.5 
3.Certificate: ISO9001/ISO14001 
4.rubber: IIR, CR, EPDM, NR, NBR

5.Connect: flange

2. Rubber expansion Joint Description:


  • The rubber expansion joint could primarily reduce the vibration and the noise of the piping system.completely solve the different piping problems as dispalcement of joint,axial flex and etc.

  • According to different material requirment ,rubber expansion joint could be made as acid proof,alkali proof,corrosion proof to suit different medium and enviroment.

  •  The material are good sealing ,light weighting,easy to fix and maintain,also has longworking expecting.. But please keep the rubber expansion  joint far away from sharp matal in order to avoid breaking of the rubber body..


  • 3. Rubber expansion Joint Physical and Mechanical:

    Physical and Mechanical Properties of Rubber Expansion Joint

    No.

    Item

    index

    Measured value

    Inner/outer 
    rubber lining

    1

    Tensile strength (Mpa)

    ≥12

    13.5

    2

    Tensile yield (%)

    ≥450

    560

    3

    Tension set at break (%)

    ≤25

    20

    4

    Hardness (Shore A hardness)

    60±5

    60

    5

    Brittleness temperature (°C)

    ≤-30

    -40

    6

    Cohesive strength (between cord fabric) (KN/m)

    ≥2.0

    4.8

    7

    100°C*48h
    Hot air aging

    Rate of Tensile Strength Reduction

    ≤25

    15

    Rate of Ultimate Elongation Reduction

    ≤30

    20

    8

    Mass change (10%H2SO4*Room temperature) %

    ≤3

    2

    9

    Mass change (10%H2SO4*Room temperature) %

    ≤3

    2