At present, China's metal ore is in the state of deep production. Thus the hardness of minerals is very high. To work out this problem,we successfully designed a new-created conical mixing grinding pan mill which is uniquely used up the hard ore.
Main advantages of such conical mixing grinding pan mill are: Increase the weight of grinding wheel, simultaneously reduce lifting surface area.After grinding wheel's rotation, the intensity of pressure on minerals increases, reaching the purpose of increasing output(not less than 150t per 24hrs)
On the basis of original equipment,a scraper device is added to keep material layer 4-5 cm.Only under this state,swaging effect is excellent.In addition,fine material can be quickly cleaned away from
mill groove.
Main Technical Parameters: |
Type | 1500t | 1400t | 1350t | 1300t | 1200t | 1100t | 1000t | 9000t | 8500t | Roller Diameter | 1500±30 | 1400±30 | 1350±30 | 1300±30 | 1200±30 | 1100±30 | 1000±30 | 9000±30 | 8500±30 | Roller Thickness | 300 350±30 400 | 245±30 | 175±15 195±15 | Heavy 175±5 Light 140±5 | Grinding Pan Diameter | 2050 2200 | 1980 | 1980 | 1980 | 1780 | 1780 | 1680 | 1680 | 1680 | Grinding Pan Thickness | 150±15 250 | 150-100 | 150-100 | 150-100 | 100-80 | 100-80 | 100-80 | 60-45 | 60-45 | Slot width of Grinding Pan | 400 500 | 360 | 240-260 | 220-240 | 175-220 | Roller Speed | | 16-18r/min | 13-18r/min | Power Distribution | 18.5 | 15 | 13 | 13 | 7.5 | 5.5 | 4.5 | Running Speed | 960r/min | 1450r/min | Feeding Granularity | <25mm | Daily Minerals Processing (t) | Iron 90-100 | Iron 60-70 | Iron 50-60 | Iron 35-40 | Gold 8 | Gold 5 | Gold 4 | Gold 3 | Gold 2 |
|