user login

automatic powder painting line powder painting line Electrostatic Spraying Process

Min. Order: 1 Set/Sets
Payment Terms: T/T
Supply Ability: 10set/month
Place of Origin: Zhejiang

Company Profile

Location: Hangzhou, Zhejiang, China (Mainland)
Business Type: Manufacturer, Distributor/Wholesaler

Product Detail

Model No.: COLO-L
Means of Transport: Ocean
Brand Name: colo
material: metal
coating: powder coating
type: Coating Production Line
structure: Chain Conveyor
Material Feature: Fire Resistant
Voltage: 220v/110v
condition: new
After-sales Service Provided: Overseas service center available
line: gas tank color coating
Power(W): 20kw
Production Capacity: 10set/month
Packing: wood case
Delivery Date: 15-30days
Show

Product Description

automatic powder painting line

powder painting line
Electrostatic Spraying Process

1. Pretreatment

Objective:To get rid of the workpiece surface oil, dirt, rust and in theworkpiece surface generating a layer of corrosion resistance and canincrease the spraying coating adhesion "phosphating layer".

Maintechnological steps: In addition to oil, rust removal, phosphating andpassivation. The workpiece surface after treatment before not only nooil, rust, dust and the original silver luster surface generating alayer of uniform and the rough is not easy to rust grey phosphating filmand can increase the coating layer adhesion.

2. Electrostatic spraying
Objective:Powder coating evenly spray to the surface of the workpiece. Thespecial work (including easy to produce electrostatic shieldingposition) should be using the high performance electrostatic spraymolding machine to complete the painting.

Process steps:
Usingelectrostatic adsorption principle in the surface of the workpieceevenly spray on a layer of powder coating. Falling powder through therecovery system recovery and sieve used again.

3. High temperature curing

Objective:The workpiece surface of powder coating heating to the specifiedtemperature and heat preservation corresponding time, melting, flowflat, curing.

Process steps: Spraying good workpiece push curingoven, heating to the predetermined temperature (usually 185 degrees)and heat preservation corresponding time (15 minutes). Blow on take outcooling namely get finished.

4. Decoration processing

Objective:Make after electrostatic spraying after the workpiece to achieve a kindof special appearance (all kinds of wood grain, decorative pattern,such as honor).

Process steps: Finish, transfer and treatment process.

automatic powder painting linepowder painting lineElectrostatic Spraying Process
automatic powder painting linepowder painting lineElectrostatic Spraying Process

automatic powder painting linepowder painting lineElectrostatic Spraying Process

Post Buying Request