Cerium stabilized zirconia beads
Good Features as below :
1) high density than Y-TZP bead.
2)excellent wear resistance.
3)lower working cost.
Physical parameters:
Properties and technique parameters | |
Composition | 18~80% ZrO2 , 13~20% CeO2 |
Packed Density | 3.8(Φ7mm)Kg/L |
Specific Density | 5.5~6.2g/cm3 |
Hardness(Mohs) | 8.5-9 |
Elastic modulus | 200GPa |
Thermal Conductivity | 3W/m.K |
Crushing Load | ≥10 (Φ7mm) KN |
Fracture Toughness | 8.5 MPam1-2 |
Thermal expansionCoeffcient(20-400 °C) | 9 10x10 -6 / °C(20-400) |
size | 0.2-15mm |
Applications :
1, wear-resistant, corrosion-resistant products: paints, textiles, paints, coating,printing and dyeing
2, high strength, high toughness products: magnetic materials, piezoelectric ceramics, dielectric ceramics.
3, prevent pollution: medicine, food, cosmetics.
4, Ceramics: Electronic ceramics, refractory ceramics, structural ceramics.
5 superfine grinding mineral(gold, silver and so on)
Cerium stabilized zirconia grinding the proportion of referrals is the grinding of zirconia referred the largest (based on customer needs the production of products 6.1 ~ 6.20 g/cm3),
from the dynamics in terms of (EC = 1/2mv2) if the use of cerium polishing equipment stabilized zirconia grinding can be referred to a larger impact energy, thereby enhancing production efficiency;
especially for high viscosity or abrasive products with high solid and easier to show its advantages. The low viscosity of the product, as a result of the option at a fixed volume of the smaller
Cestabilized zirconia abrasive grinding surface area increased referrals, and then grinding to obtain better results.