We use a "liquid-liquid composite molding process." Main
Approach: modeling, the hammer head in the sand placed on a cavity in the partition
(Made of steel A 3), which closed the cavity is divided into two departments of the respective
Points, and set the two gating system. Cavity, respectively, to two high-chromium cast casting
25 # iron and hot metal
Carbon steel. In order to combine the two materials can be good
Together, partitions made of dovetail-shaped, so that molten iron and steel not only results
Together, but also form a mechanical bond. To this end, to consider in the modeling,
Sand under the box to make dovetail-shaped grooves, so that when the partitions can be combined in the box,
The next box 5mm deep into the sand to ensure does not occur when the steel casting
Water mixed with molten iron. It should be noted that the thickness of choice is a partition off
Key. Difficult to melt with thick, too thin easy to melt steel and iron will cause
Water, mixed, lost partition role. Diaphragm thickness is best, both
To ensure that the molten steel and iron to achieve integration, the three-body (steel, separators,
Hot metal) to form a complete casting final