Specification (mm) | Straightness and Flatness of Working Surface | Parallelism Between Working Surfaces |
Accuracy Grade (μm) |
0 | 1 | 2 | 0 | 1 | 2 |
500×35 | 3 | 6 | 12 | 4.5 | 9 | 18 |
750×40 | 4 | 8 | 15 | 6 | 12 | 25 |
1000×50 | 5 | 10 | 20 | 7.5 | 15 | 30 |
1250×50 | | 12 | 24 | | 18 | 36 |
1600×70 | | 15 | 30 | | 20 | 40 |
2000×80 | | 18 | 36 | | 27 | 54 |
2500×80 | | | 44 | | | 65 |
3000×100 | | | 52 | | | 78 |
3500×100 | | | 60 | | | 90 |
4000×100 | | | 68 | | | 100 |
Specification (mm) | Straightness and Flatness of Working Surface | Parallelism Between Working Surfaces |
Accuracy Grade (μm) |
0 | 1 | 2 | 0 | 1 | 2 |
500×35 | 3 | 6 | 12 | 4.5 | 9 | 18 |
750×40 | 4 | 8 | 15 | 6 | 12 | 25 |
1000×50 | 5 | 10 | 20 | 7.5 | 15 | 30 |
1250×50 | | 12 | 24 | | 18 | 36 |
1600×70 | | 15 | 30 | | 20 | 40 |
2000×80 | | 18 | 36 | | 27 | 54 |
2500×80 | | | 44 | | | 65 |
3000×100 | | | 52 | | | 78 |
3500×100 | | | 60 | | | 90 |
4000×100 | | | 68 | | | 100 |